Pre-Qualified GMAW Fillet Welding Procedure.
Fully tested, complete with Procedure Qualification Record (PQR), Welding Procedure Specification (WPS), NATA Accredited Testing Results and Material Certifications.
This Welding Procedure was specifically written for Butt Welding SHS and also works on up to 9mm plate.
| Standard | AS/NZS 1554.1 SP |
| Process | GMAW |
| Material Type | (Mild Steel) Grade 450 and Below |
| Material Thickness | 2.5mm to 9mm |
| Welded from | Single Sided Weld |
| Welding Position | 1G, 1GR, 2G |
| Backing Gas | Argon Mix |
* Notes:
This Welding Procedure has been developed by an AS1796 Cert 10 Welding Supervisor
This WPS meets the requirements of the essential variables of AS/NZS 1554.1
This Welding Procedure is pre-qualifed to AS/NZS1554.1 2014 under clause 4.4 "Portability of Qualified Welding Procedures"
A Welder Qualification test (macro) is required to ensure adequate equipment and facilities under clause 4.4(b)
More information can be found on our Welding Procedure page.
GMAW SHS Side Butt Welding Procedure - 1G, 2G - AS/NZS1554.1SP
- Brands Elite Engineering WA
- Product Code: GMAW-06
- Availability: In Stock
-
$385.00
- Ex Tax: $350.00
Available Options
Related Products
Welding Procedure Sample Plate
Our welding procedure sample plates are supplied complete with material certification ready to run y..
$38.50 Ex Tax: $35.00
Welder Qualification Sample Plate
Our welder qualification sample plates are supplied complete with material certification ready to ru..
$22.00 Ex Tax: $20.00
GMAW SHS Side Butt Welding Procedure - 1G, 2G - AS/NZS1554.1SP
Pre-Qualified GMAW Fillet Welding Procedure.Fully tested, complete with Procedure Qualification Reco..
$385.00 Ex Tax: $350.00
GMAW SHS Single Vee Butt Welding Procedure - 1G, 2G - AS/NZS1554.1SP
Pre-Qualified GMAW Fillet Welding Procedure.Fully tested, complete with Procedure Qualification Reco..
$385.00 Ex Tax: $350.00
GMAW Single Vee Butt Welding Procedure - 1G, 2G, 4G - AS/NZS1554.1SP
Pre-Qualified GMAW Single Vee Welding Procedure.Fully tested, complete with Procedure Qualification ..
$324.50 Ex Tax: $295.00
FCAW Double Vee Butt Welding Procedure - 1G, 2G, 4G - AS/NZS1554.1SP
Pre-Qualified FCAW Double Vee Welding Procedure.Fully tested, complete with Procedure Qualification ..
$324.50 Ex Tax: $295.00