• GMAW Fillet Welding Procedure - Single Pass 3F Down - AS/NZS1554.1SP

Pre-Qualified GMAW Fillet Welding Procedure.

Fully tested, complete with Procedure Qualification Record (PQR), Welding Procedure Specification (WPS), NATA Accredited Testing Results and Material Certifications.


Standard
AS/NZS 1554.1 SP
Process

GMAW

Material Type

(Mild Steel) Grade 350 and Below

Material Thickness
Unlimited
Weld Size
6mm Fillet and Below
Welding Position

3F (D) Vertical Down

Backing Gas
Argon Mix


If you require any help with selecting the correct procedure please contact us.


* Notes:
This Welding Procedure has been developed by an AS1796 Cert 10 Welding Supervisor
This WPS meets the requirements of the essential variables of AS/NZS 1554.1
This Welding Procedure is pre-qualifed to AS/NZS1554.1 2014 under clause 4.4 "Portability of Qualified Welding Procedures"
A Welder Qualification test (macro) is required to ensure adequate equipment and facilities under clause 4.4(b)

More information can be found on our Welding Procedure page.

Write a review

Note: HTML is not translated!
    Bad           Good

GMAW Fillet Welding Procedure - Single Pass 3F Down - AS/NZS1554.1SP

  • $165.00

  • Ex Tax: $150.00

Available Options


Related Products

Welding Procedure Sample Plate

Welding Procedure Sample Plate

Our welding procedure sample plates are supplied complete with material certification ready to run y..

$38.50 Ex Tax: $35.00

Welder Qualification Sample Plate

Welder Qualification Sample Plate

Our welder qualification sample plates are supplied complete with material certification ready to ru..

$22.00 Ex Tax: $20.00

FCAW Fillet Welding Procedure - Single Pass 1F,2F,4F - AS/NZS1554.1SP

FCAW Fillet Welding Procedure - Single Pass 1F,2F,4F - AS/NZS1554.1SP

Pre-Qualified GMAW Fillet Welding Procedure.Fully tested, complete with Procedure Qualification Reco..

$165.00 Ex Tax: $150.00

Tags: Fillet, GMAW, 1554.1SP, Vertial-Down