Pre-Qualified FCAW Fillet Welding Procedure.
Fully tested, complete with Procedure Qualification Record (PQR), Welding Procedure Specification (WPS), NATA Accredited Testing Results and Material Certifications.
| Standard | AS/NZS 1554.1 SP |
| Process | FCAW E71T-1 |
| Material Type | (Mild Steel) Grade 350 and Below |
| Material Thickness | Unlimited |
| Weld Size | 6mm Fillet and Below |
| Welding Position | 1F, 2F & 4F (PA, PB, PC, PD, PE) |
| Backing Gas | Carbon Dioxide |
* Notes:
This Welding Procedure has been developed by an AS1796 Cert 10 Welding Supervisor
This WPS meets the requirements of the essential variables of AS/NZS 1554.1
This Welding Procedure is pre-qualifed to AS/NZS1554.1 2014 under clause 4.4 "Portability of Qualified Welding Procedures"
A Welder Qualification test (macro) is required to ensure adequate equipment and facilities under clause 4.4(b)
More information can be found on our Welding Procedure page.
FCAW Fillet Welding Procedure - Single Pass 1F,2F,4F - AS/NZS1554.1SP
- Brands Elite Engineering WA
- Product Code: FCAW-01
- Availability: In Stock
-
$165.00
- Ex Tax: $150.00
Available Options
Related Products
GMAW Fillet Welding Procedure - Single Pass 3F Down - AS/NZS1554.1SP
Pre-Qualified GMAW Fillet Welding Procedure.Fully tested, complete with Procedure Qualification Reco..
$165.00 Ex Tax: $150.00
FCAW Fillet Welding Procedure - Single Pass 1F,2F,4F - AS/NZS1554.1SP
Pre-Qualified FCAW Fillet Welding Procedure.Fully tested, complete with Procedure Qualification Reco..
$165.00 Ex Tax: $150.00
FCAW Fillet Welding Procedure - Multi Pass 1F,2F,4F - AS/NZS1554.1SP
Pre-Qualified FCAW Fillet Welding Procedure.Fully tested, complete with Procedure Qualification Reco..
$165.00 Ex Tax: $150.00
FCAW Fillet Welding Procedure - Single Pass 3F(UP) - AS/NZS1554.1SP
Pre-Qualified FCAW Fillet Welding Procedure.Fully tested, complete with Procedure Qualification Reco..
$180.40 Ex Tax: $164.00
MMAW Fillet Welding Procedure - Single Pass 1F,2F,4F - AS/NZS1554.1SP
Pre-Qualified MMAW Fillet Welding Procedure.Fully tested, complete with Procedure Qualification Reco..
$165.00 Ex Tax: $150.00