• FCAW Fillet Welding Procedure - Multi Pass 1F,2F,4F - AS/NZS1554.1SP

Pre-Qualified FCAW Fillet Welding Procedure.

Fully tested, complete with Procedure Qualification Record (PQR), Welding Procedure Specification (WPS), NATA Accredited Testing Results and Material Certifications.


Standard
AS/NZS 1554.1 SP
Process
FCAW
Material Type
(Mild Steel) Grade 350 and Below
Material Thickness
Unlimited
Weld Size
7mm Fillet and Above
Welding Position

1F, 2F & 4F (PA, PB, PC, PD, PE)

Backing Gas
Carbon Dioxide


If you require any help with selecting the correct procedure please contact us.


* Notes:
This Welding Procedure has been developed by an AS1796 Cert 10 Welding Supervisor
This WPS meets the requirements of the essential variables of AS/NZS 1554.1
This Welding Procedure is pre-qualifed to AS/NZS1554.1 2014 under clause 4.4 "Portability of Qualified Welding Procedures"
A Welder Qualification test (macro) is required to ensure adequate equipment and facilities under clause 4.4(b)

More information can be found on our Welding Procedure page.

Write a review

Note: HTML is not translated!
    Bad           Good

FCAW Fillet Welding Procedure - Multi Pass 1F,2F,4F - AS/NZS1554.1SP

  • $165.00

  • Ex Tax: $150.00

Available Options


Related Products

Welding Procedure Sample Plate

Welding Procedure Sample Plate

Our welding procedure sample plates are supplied complete with material certification ready to run y..

$38.50 Ex Tax: $35.00

Welder Qualification Sample Plate

Welder Qualification Sample Plate

Our welder qualification sample plates are supplied complete with material certification ready to ru..

$22.00 Ex Tax: $20.00

FCAW Fillet Welding Procedure - Single Pass 1F,2F,4F - AS/NZS1554.1SP

FCAW Fillet Welding Procedure - Single Pass 1F,2F,4F - AS/NZS1554.1SP

Pre-Qualified FCAW Fillet Welding Procedure.Fully tested, complete with Procedure Qualification Reco..

$165.00 Ex Tax: $150.00

FCAW Fillet Welding Procedure - Single Pass 3F(UP) - AS/NZS1554.1SP

FCAW Fillet Welding Procedure - Single Pass 3F(UP) - AS/NZS1554.1SP

Pre-Qualified FCAW Fillet Welding Procedure.Fully tested, complete with Procedure Qualification Reco..

$180.40 Ex Tax: $164.00

Tags: Fillet, FCAW, 1554.1SP, Multi-Pass